Mechanism of improved intermediate temperature plasticity of nickel-base single crystal superalloy with hot isostatic pressing
Publication date: Available online 8 July 2021Source: Journal of Materials Research and TechnologyAuthor(s): Weidong Xuan, Zhongming Ren