Micro-galvanic corrosion behavior and mechanical properties of extruded Mg–2Y–1Zn-0.4Zr-0.3Sr alloys with different extrusion temperament immersed in simulated body fluids
Publication date: 1 October 2021Source: Materials Chemistry and Physics, Volume 271Author(s): Xin Cao, Zhengwei Zhang, Chunxiang Xu, Conglin Ren, Wenfu Yang, Jinshan Zhang
Source: Materials Chemistry and Physics - Category: Materials Science Source Type: research