Oxidation-induced rhenium evaporation in Ni-based single crystal superalloy thin lamella
Publication date: October 2021Source: Scripta Materialia, Volume 203Author(s): Yanhui Chen, Wenhan Zhang, Yunsong Zhao, Yadi Zhai, Bin Zhang, Hui Lu, Guo Yang, Luyan Yang, Ang Li