Scratch hardness at a small scale: experimental methods and correlation to nanoindentation hardness
Publication date: Available online 2 July 2021Source: Tribology InternationalAuthor(s): Hanna Tsybenko, Farnaz Farzam, Gerhard Dehm, Steffen Brinckmann
Source: Tribology International - Category: Materials Science Source Type: research