The role of shot peening on liquation cracking in laser cladding of K447A nickel superalloy powders over its non-weldable cast structure
Publication date: Available online 30 June 2021Source: Materials Science and Engineering: AAuthor(s): Zhenlin Zhang, Yue Zhao, Jiguo Shan, Aiping Wu, Yutaka S. Sato, Shun Tokita, Kota Kadoi, Hiroshige Inoue, Huaipeng Gu, Xin Tang