Microstructural evolution and stress rupture behaviour of a Ni-Based wrought superalloy during thermal exposure
Publication date: Available online 29 June 2021Source: Materials Science and Engineering: AAuthor(s): Weiwen Kong, Yongqiang Wang, Chao Yuan, Baoning Zhang