Erratum to “Microstructure and Mechanical Properties of Haynes 282 Superalloy Produced by Laser Powder Bed Fusion” [Materials Today Communications 26 (2021) 102038]
Publication date: Available online 23 June 2021Source: Materials Today CommunicationsAuthor(s): Abdul Shaafi Shaikh, Fiona Schulz, Kevin Minet-Lallemand, Eduard Hryha