Effects of solution temperatures on creep resistance in a powder metallurgy nickel-based superalloy
Publication date: Available online 19 June 2021Source: Materials Today CommunicationsAuthor(s): Zichao Peng, Jinwen Zou, Yu Wang, Lei Zhou, Yue Tang
Source: Materials Today Communications - Category: Materials Science Source Type: research