Homogenization behavior of IN 718 superalloy prepared by electron beam layered solidification technology
Publication date: July–August 2021Source: Journal of Materials Research and Technology, Volume 13Author(s): Longhai Zhao, Yi Tan, Yilin Wang, Xiaogang You, Kai Chang, Xinpeng Zhuang, Pengting Li, Yebing Hu