Influence of temperature and hydrostatic pressure on the galvanic corrosion between 90/10 Cu-Ni and AISI 316L stainless steel
Publication date: Available online 28 May 2021Source: Journal of Materials Research and TechnologyAuthor(s): Shengbo Hu, Rui Liu, Li Liu, Yu Cui, Fuhui Wang