Hot-corrosion behavior associated with the evolution of corrosion scales of a Ni-based superalloy in molten salts
Publication date: Available online 20 May 2021Source: Progress in Natural Science: Materials InternationalAuthor(s): Ruifeng Dong, Dong Liu, Tiebang Zhang, Ling Yang, Li Wu, Yuhong Zhao, Hua Hou