Grain boundary character and stress corrosion cracking behavior of Co-Cr alloy fabricated by selective laser melting
Publication date: Available online 17 May 2021Source: Journal of Materials Science & TechnologyAuthor(s): Xin Dong, Ning Li, Yanan Zhou, Huabei Peng, Yuntao Qu, Qi Sun, Haojiang Shi, Rui Li, Sheng Xu, Jiazhen Yan
Source: Journal of Materials Science and Technology - Category: Materials Science Source Type: research