Compositionally graded nano-sized borides in a directionally solidified nickel-base superalloy
Publication date: August 2021Source: Scripta Materialia, Volume 201Author(s): Richa Gupta, K.C. Hari Kumar, M.J.N.V. Prasad, Prita Pant