Microstructure and wear behavior of IC10 directionally solidified superalloy repaired by directed energy deposition
Publication date: Available online 9 May 2021Source: Journal of Materials Science & TechnologyAuthor(s): Guan Liu, Dong Du, Kaiming Wang, Ze Pu, Dongqi Zhang, Baohua Chang
Source: Journal of Materials Science and Technology - Category: Materials Science Source Type: research