Plasticity-induced stacking fault behaviors of γ’ precipitates in novel CoNi-based superalloys
Publication date: Available online 24 April 2021Source: Journal of Materials Science & TechnologyAuthor(s): W.-W. Xu, G.H. Yin, Z.Y. Xiong, Q. Yu, T.Q. Gang, L.J. Chen
Source: Journal of Materials Science and Technology - Category: Materials Science Source Type: research