A binary beta titanium superalloy containing ordered-beta TiFe, alpha and omega
Publication date: 15 July 2021Source: Scripta Materialia, Volume 200Author(s): R.D. Jones, A.J. Knowles, W.J. Clegg
Source: Scripta Materialia - Category: Materials Science Source Type: research