Strain rate shift for constitutive behaviour of sintered silver nanoparticles under nanoindentation
Publication date: Available online 14 April 2021Source: Mechanics of MaterialsAuthor(s): Xu Long, Qipu Jia, Ziyi Shen, Ming Liu, Cao Guan
Source: Mechanics of Materials - Category: Materials Science Source Type: research