Nanoindentation studies of strain rate sensitivity in bulk metallic glasses
Publication date: 1 August 2021Source: Journal of Non-Crystalline Solids, Volume 565Author(s): M.S.Z. Zhao, Z.L. Long, L. Peng
Source: Journal of Non Crystalline Solids - Category: Chemistry Source Type: research