High-temperature wetting behavior of molten Ni-based superalloy on Y2O3 ceramics with different surface microstructures
Publication date: Available online 10 February 2021Source: Journal of Materials Processing TechnologyAuthor(s): Qingling Li, Huarui Zhang, Ming Gao, Jinpeng Li, Hu Zhang
Source: Journal of Materials Processing Technology - Category: Materials Science Source Type: research