The effect of low temperature heat treatment on stress corrosion crack initiation in machined 316L stainless steel in high-temperature hydrogenated water
Publication date: 1 April 2021Source: Scripta Materialia, Volume 195Author(s): Litao Chang, Kudzanai Mukahiwa, Jonathan Duff, M. Grace Burke, Fabio Scenini
Source: Scripta Materialia - Category: Materials Science Source Type: research
More News: Materials Science