Molecular dynamics simulation of nanoindentation on c-plane sapphire
Publication date: Available online 16 December 2020Source: Mechanics of MaterialsAuthor(s): Jiaming Lin, Feng Jiang, Xipeng Xu, Jing Lu, Zige Tian, Qiuling Wen, Xizhao Lu