Comprehensive investigation of the viscoelastic properties of PMMA by nanoindentation
Publication date: Available online 27 November 2020Source: Polymer TestingAuthor(s): Petra Christöfl, Caterina Czibula, Michael Berer, Gernot Oreski, Christian Teichert, Gerald Pinter
Source: Polymer Testing - Category: Chemistry Source Type: research
More News: Chemistry | Nanotechnology