Plastic deformation mechanisms in a new Ni ‐base single crystal superalloy at room temperature
This study also provides new insights into understanding the interaction of matrix dislocations with γ′ precipitates and the relationship between the tensile strength and the activation of plastic deformation mechanisms in Ni‐base superalloys.
Source: Journal of Microscopy - Category: Laboratory Medicine Authors: P. ZHANG, Y. YUAN, Z. GAO, B. LI, G. YANG, X. SONG Tags: Original Article Source Type: research